Clicking
any heading in the main data area (at right) will scroll the page back
to this top position.
Use the following links to
jump to the associated section in the main data.
Comments
Common Names
Common Uses
Countries of Distribution
Cutting Resistance
Drying Defects
Ease of Drying
Family Name
Gluing
Grain
Heartwood Color
Kiln Drying Rate
Luster
Moulding
Movement in Service
Nailing
Natural Durability
Numerical Data
Planing
Polishing
References
Regions of Distribution
Resistance to Impregnation
Response to Hand Tools
Sapwood Color
Scientific Name
Screwing
Staining
Strength Properties
Synonyms
Texture
Trade Name
Tree Size
Varnishing
Veneering Qualities
| |
Synonyms
Vateria malabarica
Common Names
Ajakarna, Bilidupa, Damar blanche, Damar tree, Damar white, Dhup maram, Dhup white, Dhupa, Dhupa paini, Dhupa-paini, Dhupada, Dupa-mara, Gugle, Hal, Illupathla, Illupothla, Indian copal, Indian copal tree, Kondricam, Maddi dhupa, Maddi-dhupa, Malabar whie piney, Munda dupa, Munda-dhupa, Paini, Paini mara, Payani, Payin, Perum piney, Piney du malabar, Piney maram, Piney varnish tree, Piney-maram, Sal-dhupa, The piney varnish, Vallay-kungiliam, Valley kungiliam, Velapiney, Vella kondrikam, Vella-hondrikam, Vella-paine, Vella-payin, Vellai kandrikan, Vellapine, Vellapiney, Vellei kundrikam, Vellei-kuntrikam, Velthapaini, White damar tree, White dammer of Southern India, White dhup
Regions of Distribution
Oceania and S.E. Asia
Countries of Distribution
[VIEW MAP]
India
Common Uses
Boat building (general), Boxes and crates, Chemical derivatives, Flooring, Heavy construction, Joinery, Ladders, Light construction, Matches, Millwork, Mine timbers, Plywood, Plywood: veneer (marine), Toys
Heartwood Color
| Brown |
|
|
|
|
|
|
|
|
|
|
|
|
| White |
|
|
|
|
|
|
|
|
|
|
|
|
| Red |
|
|
|
|
|
|
|
|
|
|
|
|
| | | | | | | | | | | | |
| Pale brown |
|
|
|
|
|
|
|
|
|
|
|
|
| Greenish to greyish |
|
|
|
|
|
|
|
|
|
|
|
|
| Yellow to golden-yellow to orange |
|
|
|
|
|
|
|
|
|
|
|
|
| Pale red to pink |
|
|
|
|
|
|
|
|
|
|
|
|
Sapwood Color
| Red |
|
|
|
|
|
|
|
|
|
|
|
|
| White |
|
|
|
|
|
|
|
|
|
|
|
|
| Pink |
|
|
|
|
|
|
|
|
|
|
|
|
| | | | | | | | | | | | |
| White to yellow |
|
|
|
|
|
|
|
|
|
|
|
|
Grain
| Interlocked |
|
|
|
|
|
|
|
|
|
|
|
|
| Even |
|
|
|
|
|
|
|
|
|
|
|
|
| Straight |
|
|
|
|
|
|
|
|
|
|
|
|
Texture
| Medium |
|
|
|
|
|
|
|
|
|
|
|
|
| Fine |
|
|
|
|
|
|
|
|
|
|
|
|
| Coarse |
|
|
|
|
|
|
|
|
|
|
|
|
| | | | | | | | | | | | |
| Medium to coarse |
|
|
|
|
|
|
|
|
|
|
|
|
Luster
Natural Durability
| Susceptible to insect attack |
|
|
|
|
|
|
|
|
|
|
|
|
| Non-durable |
|
|
|
|
|
|
|
|
|
|
|
|
| Non-resistant to powder post beetles |
|
|
|
|
|
|
|
|
|
|
|
|
| Perishable |
|
|
|
|
|
|
|
|
|
|
|
|
| Non-resistant to termites |
|
|
|
|
|
|
|
|
|
|
|
|
| | | | | | | | | | | | |
| Non durable |
|
|
|
|
|
|
|
|
|
|
|
|
| Sapwood is susceptible to wood staining fungal attack |
|
|
|
|
|
|
|
|
|
|
|
|
| Heartwood susceptible to attack by decay fungi |
|
|
|
|
|
|
|
|
|
|
|
|
Drying Defects
| Distortion |
|
|
|
|
|
|
|
|
|
|
|
|
| Splitting |
|
|
|
|
|
|
|
|
|
|
|
|
| Checking |
|
|
|
|
|
|
|
|
|
|
|
|
Ease of Drying
| Moderately Difficult to Difficult |
|
|
|
|
|
|
|
|
|
|
|
|
| Fairly Easy |
|
|
|
|
|
|
|
|
|
|
|
|
| Rapidly |
|
|
|
|
|
|
|
|
|
|
|
|
| Slowly |
|
|
|
|
|
|
|
|
|
|
|
|
| | | | | | | | | | | | |
| Easy |
|
|
|
|
|
|
|
|
|
|
|
|
| Difficult |
|
|
|
|
|
|
|
|
|
|
|
|
Kiln Drying Rate
| Naturally dries quickly |
|
|
|
|
|
|
|
|
|
|
|
|
| Naturally dries at a moderate speed |
|
|
|
|
|
|
|
|
|
|
|
|
Tree Size
| Bole length is 20-30 m |
|
|
|
|
|
|
|
|
|
|
|
|
| Tree height is 30-40 m |
|
|
|
|
|
|
|
|
|
|
|
|
| Bole length is 10-20 m |
|
|
|
|
|
|
|
|
|
|
|
|
| Bark width is 5-10 mm |
|
|
|
|
|
|
|
|
|
|
|
|
| Bark width is 20-25 mm |
|
|
|
|
|
|
|
|
|
|
|
|
| Bark width is 15-20 mm |
|
|
|
|
|
|
|
|
|
|
|
|
| Bark width is 0-5 mm |
|
|
|
|
|
|
|
|
|
|
|
|
| Tree height is 20-30 m |
|
|
|
|
|
|
|
|
|
|
|
|
| Bark width is 10-15 mm |
|
|
|
|
|
|
|
|
|
|
|
|
| Tree height is 40-50 m |
|
|
|
|
|
|
|
|
|
|
|
|
| Trunk diameter is 150-200 cm |
|
|
|
|
|
|
|
|
|
|
|
|
Comments
General finishing qualities are rated as good
Cutting Resistance
| Easy to saw |
|
|
|
|
|
|
|
|
|
|
|
|
| | | | | | | | | | | | |
| Cutting Resistance with dry wood is easy |
|
|
|
|
|
|
|
|
|
|
|
|
Gluing
Moulding
Movement in Service
| Unstable with Poor Stability - Large Movement |
|
|
|
|
|
|
|
|
|
|
|
|
Nailing
Planing
Resistance to Impregnation
| Permeable heartwood |
|
|
|
|
|
|
|
|
|
|
|
|
| Permeable sapwood |
|
|
|
|
|
|
|
|
|
|
|
|
| | | | | | | | | | | | |
| Heartwood is highly resistant |
|
|
|
|
|
|
|
|
|
|
|
|
Response to Hand Tools
| Easy to Work |
|
|
|
|
|
|
|
|
|
|
|
|
| | | | | | | | | | | | |
| Easy to machine |
|
|
|
|
|
|
|
|
|
|
|
|
Screwing
Veneering Qualities
| Suitable for peeling |
|
|
|
|
|
|
|
|
|
|
|
|
| Veneers easily |
|
|
|
|
|
|
|
|
|
|
|
|
| Veneers moderately easy |
|
|
|
|
|
|
|
|
|
|
|
|
| Difficult to veneer |
|
|
|
|
|
|
|
|
|
|
|
|
| Suitable for slicing |
|
|
|
|
|
|
|
|
|
|
|
|
Polishing
| Fair to Good Results |
|
|
|
|
|
|
|
|
|
|
|
|
| Very Good to Excellent Results |
|
|
|
|
|
|
|
|
|
|
|
|
Staining
| Very Good to Excellent Results |
|
|
|
|
|
|
|
|
|
|
|
|
| Fair to Good Results |
|
|
|
|
|
|
|
|
|
|
|
|
Varnishing
| Fair to Good Results |
|
|
|
|
|
|
|
|
|
|
|
|
| Very Good to Excellent Results |
|
|
|
|
|
|
|
|
|
|
|
|
| Fairly Easy to Very Easy |
|
|
|
|
|
|
|
|
|
|
|
|
Strength Properties
| Density (dry weight) = 31-37 lbs/cu. ft. |
|
|
|
|
|
|
|
|
|
|
|
|
| Modulus of Elasticity (stiffness) = medium |
|
|
|
|
|
|
|
|
|
|
|
|
| Max. crushing strength = medium |
|
|
|
|
|
|
|
|
|
|
|
|
| Density (dry weight) = 38-45 lbs/cu. ft. |
|
|
|
|
|
|
|
|
|
|
|
|
| Toughness-Hammer drop (Impact Strength) = very low |
|
|
|
|
|
|
|
|
|
|
|
|
| Toughness-Hammer drop (Impact Strength) = low |
|
|
|
|
|
|
|
|
|
|
|
|
| Shrinkage, Tangential = large |
|
|
|
|
|
|
|
|
|
|
|
|
| Shrinkage, Radial = small |
|
|
|
|
|
|
|
|
|
|
|
|
| Bending strength (MOR) = medium |
|
|
|
|
|
|
|
|
|
|
|
|
| Bending strength (MOR) = low |
|
|
|
|
|
|
|
|
|
|
|
|
Numerical Data
| Item | Green | Dry | English |
| | | |
| Bending Strength | 7711 | 12078 | psi |
| Density | | 35 | lbs/ft3 |
| Impact Strength | | 22 | inches |
| Maximum Crushing Strength | 3324 | 5570 | psi |
| Stiffness | 1665 | 1923 | 1000 psi |
| Weight | 34 | 27 | lbs/ft3 |
| Radial Shrinkage | 3 | | % |
| Tangential Shrinkage | 10 | | % |
| | | |
| Item | Green | Dry | Metric |
| | | |
| Bending Strength | 542 | 849 | kg/cm2 |
| Density | | 560 | kg/m3 |
| Impact Strength | | 55 | cm |
| Maximum Crushing Strength | 233 | 391 | kg/cm2 |
| Stiffness | 117 | 135 | 1000 kg/cm2 |
| Weight | 544 | 432 | kg/m3 |
| Radial Shrinkage | 3 | | % |
References
Bourdillon, T.F.,1908,The Forest Trees of Travancore,Travancore Government Press
Fundter, J.M.,1982,Names for Dipterocarp timbers and trees from Asia,Pudoc, Wageningen, Netherlands
Gamble, J.S.,1902,A Manual of Indian Timbers,Sampson Low, Marston & Co. London
Kadambi, K.,1957,Vateria indica Lina,Indian Forester 83(5) pp317-23
Nazma,1981,A handbook of Kerala Timbers,Kerala Forest Research Institute Research Report, No.9
Pearson, R.S., Brown, H.P.,1932,Commercial Timbers of India,Govt. Printer Calcutta,2 vols
Sekhar, A.C.,1967,Some Indian Timbers Equivalent to Foreign Timbers,Van Vigyan 5(1&2,pp18-24
Sweet, C.V.,1922,Further experiments in the air-seasoning of Indian timbers and general,recommendations as to seasoning methods.,Indian Forest Records IX part V, Delhi, India
Tewari, M.C., Jain, J.C.,1980,Utilization of Secondary Species,Journal of the National Building Organization 25(2) pp1-6
|
|