Clicking
any heading in the main data area (at right) will scroll the page back
to this top position.
Use the following links to
jump to the associated section in the main data.
Boring
Common Names
Common Uses
Countries of Distribution
Cutting Resistance
Drying Defects
Family Name
Grain
Heartwood Color
Kiln Drying Rate
Kiln Schedules
Luster
Mortising
Moulding
Movement in Service
Nailing
Natural Durability
Numerical Data
Planing
Polishing
References
Regions of Distribution
Resistance to Impregnation
Resistance to Splitting
Response to Hand Tools
Sapwood Color
Scientific Name
Strength Properties
Texture
Toxicity
Trade Name
Tree Identification
| |
Common Names
Allanblackia, Mkange, Mkanya, Mkanye, Msambu, Mwaka
Regions of Distribution
Africa
Countries of Distribution
[VIEW MAP]
Tanzania
Common Uses
Agricultural implements, Boxes and crates, Cabinetmaking, Flooring: industrial heavy traffic, Furniture, Joinery, Light construction, Particleboard, Piling, Plywood, Toys, Turnery, Veneer
Heartwood Color
Sapwood Color
Grain
Texture
Luster
Natural Durability
| Perishable |
|
|
|
|
|
|
|
|
|
|
|
|
| Susceptible to attack from powder post (Lyctid & Bostrychid) beetles |
|
|
|
|
|
|
|
|
|
|
|
|
| Non durable |
|
|
|
|
|
|
|
|
|
|
|
|
Toxicity
Kiln Schedules
| UK=A US=T2D4/T2D3 Fr=1 |
|
|
|
|
|
|
|
|
|
|
|
|
| Kiln Drying Rate (in days) is fairly rapid |
|
|
|
|
|
|
|
|
|
|
|
|
| Dry at a slow speed |
|
|
|
|
|
|
|
|
|
|
|
|
Drying Defects
| Slight end splitting |
|
|
|
|
|
|
|
|
|
|
|
|
| Severe cupping |
|
|
|
|
|
|
|
|
|
|
|
|
| Slight surface checking |
|
|
|
|
|
|
|
|
|
|
|
|
Kiln Drying Rate
| Fairly rapid (11-17 days for boards under 32 mm, to 31-51 days for boards greater than 63 mm) |
|
|
|
|
|
|
|
|
|
|
|
|
Tree Identification
| Bole/stem form is buttressed |
|
|
|
|
|
|
|
|
|
|
|
|
| Bole/stem form is straight |
|
|
|
|
|
|
|
|
|
|
|
|
Boring
Cutting Resistance
| Cutting Resistance with dry wood is moderate |
|
|
|
|
|
|
|
|
|
|
|
|
Mortising
| Moderately easy to mortise |
|
|
|
|
|
|
|
|
|
|
|
|
| Finishes satisfactorily |
|
|
|
|
|
|
|
|
|
|
|
|
Moulding
| Satisfactory moulding results |
|
|
|
|
|
|
|
|
|
|
|
|
| Moulding ease is moderate |
|
|
|
|
|
|
|
|
|
|
|
|
| Good finishing results |
|
|
|
|
|
|
|
|
|
|
|
|
Movement in Service
| Not stable/prone to move |
|
|
|
|
|
|
|
|
|
|
|
|
| Large |
|
|
|
|
|
|
|
|
|
|
|
|
Nailing
Planing
| Planes to a satisfactory finish |
|
|
|
|
|
|
|
|
|
|
|
|
| Ease of planing is moderate |
|
|
|
|
|
|
|
|
|
|
|
|
Resistance to Impregnation
| Sapwood is permeable |
|
|
|
|
|
|
|
|
|
|
|
|
| Heartwood is extremely resistant |
|
|
|
|
|
|
|
|
|
|
|
|
Resistance to Splitting
Response to Hand Tools
| Easy to Work |
|
|
|
|
|
|
|
|
|
|
|
|
| | | | | | | | | | | | |
| Easy to machine |
|
|
|
|
|
|
|
|
|
|
|
|
Polishing
| Very Good to Excellent Results |
|
|
|
|
|
|
|
|
|
|
|
|
| Fair to Good Results |
|
|
|
|
|
|
|
|
|
|
|
|
| | | | | | | | | | | | |
| Good results |
|
|
|
|
|
|
|
|
|
|
|
|
Strength Properties
| Density (dry weight) = 46-52 lbs/cu. ft. |
|
|
|
|
|
|
|
|
|
|
|
|
| Max. crushing strength = medium |
|
|
|
|
|
|
|
|
|
|
|
|
| Bending strength (MOR) = medium |
|
|
|
|
|
|
|
|
|
|
|
|
| Density (dry weight) = 38-45 lbs/cu. ft. |
|
|
|
|
|
|
|
|
|
|
|
|
| Shearing strength (parallel to grain) = low |
|
|
|
|
|
|
|
|
|
|
|
|
| Modulus of Elasticity (stiffness) = medium |
|
|
|
|
|
|
|
|
|
|
|
|
| Shrinkage, Tangential = fairly large |
|
|
|
|
|
|
|
|
|
|
|
|
| Shrinkage, Radial = very small |
|
|
|
|
|
|
|
|
|
|
|
|
| Shearing strength (parallel to grain) = medium |
|
|
|
|
|
|
|
|
|
|
|
|
| Modulus of Elasticity (stiffness) = low |
|
|
|
|
|
|
|
|
|
|
|
|
| Hardness (side grain) = soft |
|
|
|
|
|
|
|
|
|
|
|
|
| Bending strength (MOR) = low |
|
|
|
|
|
|
|
|
|
|
|
|
| Toughness (total work) = low |
|
|
|
|
|
|
|
|
|
|
|
|
| Shrinkage, Tangential = large |
|
|
|
|
|
|
|
|
|
|
|
|
| Shrinkage, Radial = small |
|
|
|
|
|
|
|
|
|
|
|
|
| Shearing strength (parallel to grain) = very low |
|
|
|
|
|
|
|
|
|
|
|
|
| Max. crushing strength = high |
|
|
|
|
|
|
|
|
|
|
|
|
Numerical Data
| Item | Green | Dry | English |
| | | |
| Bending Strength | 8397 | 13144 | psi |
| Density | | 45 | lbs/ft3 |
| Hardness | | 995 | lbs |
| Maximum Crushing Strength | 4413 | 6988 | psi |
| Shearing Strength | | 1662 | psi |
| Stiffness | 1543 | 1781 | 1000 psi |
| Toughness | | 167 | inch-lbs |
| Weight | 44 | 35 | lbs/ft3 |
| Radial Shrinkage | 2 | | % |
| Tangential Shrinkage | 9 | | % |
| | | |
| Item | Green | Dry | Metric |
| | | |
| Bending Strength | 590 | 924 | kg/cm2 |
| Density | | 721 | kg/m3 |
| Hardness | | 451 | kg |
| Maximum Crushing Strength | 310 | 491 | kg/cm2 |
| Shearing Strength | | 116 | kg/cm2 |
| Stiffness | 108 | 125 | 1000 kg/cm2 |
| Toughness | | 192 | cm-kg |
| Weight | 705 | 560 | kg/m3 |
| Radial Shrinkage | 2 | | % |
References
Banks, C.H. and J.P. Schoeman. 1963. Railway Sleeper and Crossing Timbers. Bulletin No. 41, Republic of South Africa. The Government Printer, Pretoria, South Africa.
Banks, C.H., Schoeman, J.P., Otto, K.P.,1977,The Mechanical Properties of Timbers with particular reference to South,Africa,South African Forestry Research Institute Bulletin,(Ed.,Schoeman, J.P. 1973 & Otto K.P. 1976,No.48
Bolza, E., Keating, W.G.,1972,African Timbers - the Properties, Uses and Characteristics of 700 Species,C.S.I.R.O. Div. of Building Research
Murira, K.,1984,Natural Durability Tests of Tanzanian Timbers 1955 - 1982,Tanzania Forestry Research Institute, Timber Utilisation Research Centre,,Moshi.
Takahashi, A.,1978,Compilation of Data on the Mechanical Properties of Foreign Woods (Part,III) Africa,Shimane University, Japan, Research Report on Foreign Wood No. 7
Tanzania Forest Department,1960,The Natural Durability of Local Timbers,Tanzanian Forest Dept. Tech. Note,No.14
Tanzania Forest Division,1966,Kiln Drying Schedules for Tanzania Timbers Technical Note no.38,Tanzania Forest Div. Util. Sec. Moshi
Tanzania Forestry Department,1961,Timbers of Tanganyika - Allanblackia stuhlmannii (mkanya, msambu,Tanzania Forestry Department, Utilisation Section, Moshi - Timbers of,Tanganyika
|
|